Sample: AM50_2p5 ST Ungroup Processes
Last Updated: 2 days ago Owner: Tracy Berman ID: 67424
EPMA Data Collection (4)
Date:
42557
Date:
42655
Date:
42293
Region of interest:
near edge
Region of interest:
edge
Region of interest:
center
Elements Measured:
Mg, Al, Zn, Mn
number of measurements made:
50
number of measurements made:
49
data start row:
401
data start row:
51
data start row:
100
data end row:
450
data end row:
99
data end row:
148
Measurements
Alloy Name:
AM50
Plate Thickness:
2.5 mm
Composition Al Content:
4.6 wt %
Composition Mn Content:
0.41 wt %
Composition Mg Content:
94.99 wt %
Files
EPMA WIRS Analysis (3)
Date:
10/24/2016
Region of Interest:
Near Edge
Region of Interest:
Edge
Region of Interest:
Center
Measurements
Alloy Name:
AM50
Plate Thickness:
2.5 mm
Composition Al Content:
4.6 wt %
Composition Mn Content:
0.41 wt %
Composition Mg Content:
94.99 wt %
Files
Received As-Cast Plates (1)
Measurements
Alloy Name:
AM50
Plate Thickness:
2.5 mm
Composition Al Content:
4.6 wt %
Composition Mn Content:
0.41 wt %
Composition Mg Content:
94.99 wt %
Solution Treatment (1)
Temperature:
420 ÂșC
Time:
2 h
Quench:
water
Measurements
Alloy Name:
AM50
Plate Thickness:
2.5 mm
Composition Al Content:
4.6 wt %
Composition Mn Content:
0.41 wt %
Composition Mg Content:
94.99 wt %